The learner will demonstrate knowledge of flux cored arc welding terminology and defects.
Two similar types of incomplete fusion to the base metal are called cold lap and ______________.
Two similar types of incomplete fusion to the base metal are called cold lap and ______________.
overlap
Two similar types of incomplete fusion to the base metal are called cold lap and ______________.
overlap
A crack at the end of the weld is called a:
A crack at the end of the weld is called a:
crater crack
Porosity in a straight line is called aligned porosity. What is it called if the porosity is all over the weld?
Porosity in a straight line is called aligned porosity. What is it called if the porosity is all over the weld?
Scattered Porosity
Porosity in a straight line is called aligned porosity. What is it called if the porosity is all over the weld?
Scattered Porosity
Excessive electrode extension requires an increase in what to adequately blanket the weld pool:
Excessive electrode extension requires an increase in what to adequately blanket the weld pool:
shielding gas
Excessive electrode extension requires an increase in what to adequately blanket the weld pool:
shielding gas
Round scattered droplets of weld metal that are unsightly and may lead to stress riser cracking is:
Round scattered droplets of weld metal that are unsightly and may lead to stress riser cracking is:
spatter
Round scattered droplets of weld metal that are unsightly and may lead to stress riser cracking is:
spatter
With an improper work angle you will likely end up with ______________ or incomplete penetration.
With an improper work angle you will likely end up with ______________ or incomplete penetration.
incomplete fusion
With an improper work angle you will likely end up with ______________ or incomplete penetration.
incomplete fusion
To reduce surface tension, the mill scale could be ground off or the use of ____________ also helps.
To reduce surface tension, the mill scale could be ground off or the use of ____________ also helps.
argon shielding gas
To reduce surface tension, the mill scale could be ground off or the use of ____________ also helps.
argon shielding gas
An unacceptable flaw is called a _______________.
An unacceptable flaw is called a _______________.
defect
Identify what "B" represents.
Electrode Extension
If the base metal at the toes of the weld are melted away, the defects or discontinuities are called ______________.
If the base metal at the toes of the weld are melted away, the defects or discontinuities are called ______________.
undercut
If the base metal at the toes of the weld are melted away, the defects or discontinuities are called ______________.
undercut
Undercutting and an unstable arc are more problematic with which type of shielding gas?
Undercutting and an unstable arc are more problematic with which type of shielding gas?
100% Carbon Dioxide
Undercutting and an unstable arc are more problematic with which type of shielding gas?
100% Carbon Dioxide
If the electrode wire is rusty on the spool, ______________ may result.
If the electrode wire is rusty on the spool, ______________ may result.
porosity
If the electrode wire is rusty on the spool, ______________ may result.
porosity